Material | density (g/cm3) | X-ray energy (keV) | X-ray wavelength (Å) | critical angle (°) | qc (Å−1) | SLD (10−6Å−2) |
---|---|---|---|---|---|---|
Silicon | 2.33 | 8.0 | 1.54 | 0.223 | 0.0318 | 20.07 |
13.5 | 0.92 | 0.132 | 0.0316 | 19.88 | ||
SiO2 | 2.65 | 8.0 | 1.54 | 0.238 | 0.0338 | 22.70 |
13.5 | 0.92 | 0.141 | 0.0337 | 22.56 | ||
Aluminium oxide | 3.95 | 8.0 | 1.54 | 0.287 | 0.0409 | 33.25 |
13.5 | 0.92 | 0.171 | 0.0408 | 33.04 | ||
PMMA | 1.18 | 8.0 | 1.54 | 0.164 | 0.0233 | 10.84 |
13.5 | 0.92 | 0.098 | 0.0233 | 10.81 | ||
polystyrene | 1.06 | 8.0 | 1.54 | 0.155 | 0.0221 | 9.70 |
13.5 | 0.92 | 0.092 | 0.0221 | 9.68 | ||
PS-b-PMMA 75:25 | 1.09 | 8.0 | 1.54 | 0.157 | 0.0224 | 9.98 |
13.5 | 0.92 | 0.094 | 0.0224 | 9.96 | ||
PS-b-PMMA 50:50 | 1.12 | 8.0 | 1.54 | 0.160 | 0.0227 | 10.27 |
13.5 | 0.92 | 0.095 | 0.0227 | 10.25 | ||
Vacuum (or air) | 0 | 8.0 | 1.54 | 0 | 0 | 0 |
13.5 | 0.92 | 0 | 0 | 0 |