Extra:SLD examples

From GISAXS
Revision as of 15:02, 23 April 2019 by KevinYager (talk | contribs) (Created page with " {| class="wikitable" |- ! Material ! density (g/cm<sup>3</sup>) ! X-ray energy (keV) ! X-ray wavelength (Å) ! critical angle (°) ! ''q<sub>c</sub>'' (Å<sup>−1</sup>) ! S...")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to: navigation, search
Material density (g/cm3) X-ray energy (keV) X-ray wavelength (Å) critical angle (°) qc−1) SLD (10−6Å−2)
Silicon 2.33 8.0 1.54 0.223 0.0318 20.07
13.5 0.92 0.132 0.0316 19.88
SiO2 2.65 8.0 1.54 0.238 0.0338 22.70
13.5 0.92 0.141 0.0337 22.56
Aluminium oxide 3.95 8.0 1.54 0.287 0.0409 33.25
13.5 0.92 0.171 0.0408 33.04
PMMA 1.18 8.0 1.54 0.164 0.0233 10.84
13.5 0.92 0.098 0.0233 10.81
polystyrene 1.06 8.0 1.54 0.155 0.0221 9.70
13.5 0.92 0.092 0.0221 9.68
PS-b-PMMA 75:25 1.09 8.0 1.54 0.157 0.0224 9.98
13.5 0.92 0.094 0.0224 9.96
PS-b-PMMA 50:50 1.12 8.0 1.54 0.160 0.0227 10.27
13.5 0.92 0.095 0.0227 10.25
Vacuum (or air) 0 8.0 1.54 0 0 0
13.5 0.92 0 0 0